Skip to content

pei

1 post with the tag “pei”

OrcaSlicer Bed Type Settings: All Six Plates Explained

Open the Bed type dropdown in OrcaSlicer and you get six options. None of them says “smooth PEI” — and a smooth PEI sheet is the most common plate in the hobby. If that is what is on your printer, the setting you want is Smooth High Temp Plate, and nothing in that name tells you so.

That is the short version. Orca slicer build plate settings are the most-ignored corner of the slicer, and the Orca bed type control is doing more work than its one-line label suggests. Here is the rest of it: where the setting lives in both OrcaSlicer and Elegoo Slicer, what all six plates are for, what bed temperature to run on each, and why this dropdown changes more than a label.

Grab the reference sheet. Everything below is condensed into a three-page PDF you can keep next to the printer — all six plates, a bed temp matrix by material, and the sources behind every number. Download the OrcaSlicer bed types reference (PDF)

The full orca slicer change bed type workflow is four steps:

  1. Open the Prepare tab.
  2. Find the Bed type selector near the plate in the right-hand panel.
  3. Pick the plate that is physically on your printer right now — not the one the printer profile shipped with.
  4. Re-slice.

That last step matters more than it looks, and the next section explains why.

If you want per-plate temperatures to actually apply, you also need Support multi bed types enabled in Printer Settings. With that off, the per-plate temperature fields are not in play.

Elegoo Slicer is an OrcaSlicer fork, so the answer to elegoo slicer change bed type is the same answer: same control, same place on the Prepare tab, same behaviour. Anything in this post about orca slicer plate settings applies there too.

Creality Slicer is also Orca-derived, with one addition — it carries an Epoxy Resin Plate option that upstream OrcaSlicer does not have, for Creality’s double-sided epoxy-coated sheet. Creality publishes no temperature figures for it.

Dropdown option What it physically is Best for
Smooth Cool Plate Low-temperature coated sheet, glossy finish PLA at low bed temps, glossy first layers
Textured Cool Plate The same coated sheet, textured finish PLA at low bed temps, matte first layers
Cool Plate (SuperTack) High-grip low-temperature surface PLA and PETG with no glue at all
Smooth High Temp Plate This is the smooth PEI plate Glossy first layers on bare PEI
Textured PEI Plate Powder-coated PEI on spring steel The all-rounder — widest material list
Engineering Plate High-temperature engineering surface ABS, ASA, PC, PA, PA-CF

Two things worth knowing about that list.

The two Cool Plate entries are the same surface. Smooth Cool Plate and Textured Cool Plate differ in finish only — same coating, same temperature guidance, same glue habit. Pick whichever matches the sheet in your hand and stop worrying about it.

Cool Plate (SuperTack) is a genuinely different plate, not a variant of the above. It is a high-grip surface intended to hold PLA and PETG without any glue stick at all. Clean it with warm water and detergent — not IPA.

The naming trap: your smooth PEI plate is called something else

Section titled “The naming trap: your smooth PEI plate is called something else”

This is the part that trips people up, and it is why orca slicer bed type gets searched as often as it does.

Of the six options, exactly one contains the letters PEI — Textured PEI Plate. So if you have a smooth PEI sheet on your printer, you scan the list, see nothing that matches, and leave the dropdown wherever the profile put it.

The right answer is Smooth High Temp Plate. It is the smooth PEI plate. The name describes its temperature rating rather than its surface, which is technically accurate and practically useless when you are looking for the word “PEI.”

Published sources put the smooth PEI plate’s ceiling at around 120 °C, against 180 °C for the textured PEI plate. If you print a lot of high-bed-temperature materials, that difference is worth knowing independently of which dropdown entry you pick.

Here is the thing most guides skip. The bed type dropdown is not cosmetic.

Every filament profile stores a separate bed temperature per plate type, with independent values for the first layer and all other layers. The dropdown decides which of those stored pairs gets written into your G-code.

Prove it to yourself in about ninety seconds:

  1. Slice any model. Open the G-code preview and note the bed temperature.
  2. Change the bed type. Nothing else.
  3. Re-slice. Look at the bed temperature again.

The M140 / M190 value changes. Which means if the dropdown is wrong, your first layer is being printed at a temperature you never chose — and “my first layer won’t stick” turns out to have been a settings problem the whole time.

This is also why there is no separate orca slicer change bed temp procedure to learn. You can override the number directly in Filament Settings, but the plate you select is what decides which stored value gets used in the first place. Fix the bed type and the temperature usually fixes itself.

Here is where I have to be straight with you: the published sources do not agree, and pretending otherwise would make this post less useful, not more.

Material Bambu spec (Textured PEI) OrcaSlicer wiki Kingroon (smooth PEI)
PLA 45–60 °C 50–60 °C 70 °C
PETG 60–80 °C not listed 70 °C
ABS 90–100 °C 90–100 °C —
ASA 90–100 °C 90–100 °C —
TPU 35–45 °C 40–60 °C —
PC 90–110 °C 100–120 °C —
PA / Nylon 90–110 °C 90–110 °C —

Three sources, and a 25 °C spread on PLA — the most common filament there is. OrcaSlicer’s own material temperature table omits PETG entirely. ABS and ASA are the only rows where everyone agrees outright.

There is no version of this where a chart hands you the right number. Use the spread as a sanity check, then print a first-layer patch and decide by looking at it.

The glue question is equally muddled. Bambu’s own specification lists PETG as needing no adhesive on textured PEI; other guides say a glue stick is necessary there precisely because adhesion is otherwise too strong. Bambu’s Cool Plate wiki recommends a thin glue coat every two or three prints. Pick a position based on your own plates, not on a table.

You will see it repeated everywhere that PETG bonds aggressively to bare smooth PEI — strongly enough that removing a part can take coating with it. All3DP’s guidance is that PETG, TPU and PC “can stick too strongly to smooth PEI, so a release layer may be needed.”

I have not damaged a plate this way and I am not going to show you photos of something I have not seen. What I will say is that the precaution is cheap: run PETG on textured PEI, or put a glue stick down as a release layer if you want the glossy bottom. There is no upside to finding out the hard way.

First layer settings that change with the plate

Section titled “First layer settings that change with the plate”

Bed temperature is stored per plate. Most other first-layer settings are not — which means these are the ones you change by hand every time you swap:

  • Z-offset — plates are not all the same thickness
  • First layer flow — a textured surface has valley volume to fill that a smooth one does not
  • Elephant foot compensation — behaves differently on textured vs. smooth
  • First layer speed

If you own more than one plate, the honest advice is to keep a saved printer profile per plate rather than trying to remember which numbers went with which sheet.

OrcaSlicer passes the selected plate to your machine start G-code as curr_bed_type, so the offset can travel with the plate instead of being changed by hand:

{if curr_bed_type=="Textured PEI Plate"}
SET_GCODE_OFFSET Z=-0.05
{else}
SET_GCODE_OFFSET Z=0.0
{endif}

The string has to match the dropdown entry exactly, including case — the same names as the table above. The -0.05 is an example, not a value to copy: calibrate it against your own first layer on that plate.

For an aftermarket sheet — a third-party PEI sheet, a garolite plate, a textured spring steel that did not come with the machine — pick the option whose surface and temperature range most closely matches what you actually have, then set your bed temperature by test rather than trusting the preset. The dropdown is a starting point, not a driver.

Aftermarket plates also carry their own ratings that have nothing to do with the dropdown entry you pick. QIDI’s Cool Plate Pro, for example, publishes a 120 °C surface temperature resistance and a material list running up to PPS and PPA — a very different plate from the Bambu-lineage Cool Plate that OrcaSlicer’s entry is named after. Read your plate’s own documentation.

Check my working. Every figure in this post is a published number from one of these, cross-checked against the others and attributed wherever they conflict.

None of it has been measured on your printer, and where I have tested something myself I have said so. If a number here disagrees with your machine, your machine is right.


Download the three-page reference PDF · Watch the video · More free 3D printing calculators · Free Klipper configs

No sponsored printer reviews. Ever.